IrO2 Coated Titanium Anode

No.GH09002
IrO2 coated on titanium surface by sintering.
Substrate
Pure Titanium
Coating
IrO2
Size
Customized
Type
Plate,Bar, Mesh, Tube, Wire etc.
Application
Electroplating, Sewage treatment, Producing Hydrogen, Copper recovery etc.
Inspection
Strength Working Life Test
Trade Item
EXW, DDU, DDP, DAP, CIF, etc
Cargo Service
Express, by Flight, by Sea, by Train(truck)
Working Life
depend on the anode working condition, professional engineer will advise the guaranteed working life
Payment Method
TT or Negotiable
  • IrO2 Coated Titanium Anode
  • IrO2 Coated Titanium Anode
  • IrO2 Coated Titanium Anode
  • IrO2 Coated Titanium Anode

Description

IrO2 Coated Titanium Anode is widely to be used in oxygen evolution reaction. Such as kinds of industries as follow:
Titanium anode for electroplating industry
Titanium anode for aluminum foil for aluminum foil conversion
Titanium anode etching solution for copper recovery
Titanium anode for electrolytic copper foil,
Titanium anode for cyclone electrolysis equipment
Titanium anode for cathodic protection

The features of IrO2 coated titanium anode:
1. Extremely high anti-corrosion performance;
2. High current efficiency, Oxygen evolution overpotential ≤ 1 5V (relative to calomel electrode);
3. Long working life and high electrocatalytic oxidation activity;
4. After the electrode loses its activity, the substrate can be reused;
5. Capable of carrying high current density and high production efficiency.

Application:
metal foil, electrolytic copper foil, steel plate galvanizing, cathodic protection, organic matter electrolytic synthesis, chromium electroplating, etching solution regeneration and copper recovery, cyclone electrolysis, wet metallurgy, HHO generator, sewage treatment, etc

1,Example of an annual production of 100000 tons of electrolytic manganese project (chloride ion less than 200ppm)
Current density: 370-420A/m2
Consumption per Ton: 5800-6000KWh
Output:3.7-4.0kg/item
Working life: 36 months
Under the same working condition, lead anode can only use 18months and its output is lower than mmo anode.

2,Example of an annual production of 50000 tons of electrolytic manganese project (chloride ion less than 500ppm)
Current density: 100-230A/m2
Cell voltage: 3.6-3.7v
Current efficiency:93-95%
Working life: more than 36 months
Under the same working condition, lead anode can only use 18months and its current efficiency is lower than mmo anode.